dc.description.abstractThis article presents the results of improvement in the electrochemical properties of porous type anodic films grown on aluminium alloy AA2024 T3, obtained with the techniques of direct current, pulsed direct current and reverse pulse current, through an electrolyte H2SO4 al 15% v/v. Morphological analysis was used atomic force microscopy and scanning electron microscopy allowing to identify the films obtained with inverse pulse current have a grain size smaller than those obtained by the two other deposition techniques. The evaluation of corrosion resistance in the films, we used electrochemical impedance spectroscopy and anodic polarization curves Tafel. These evaluation techniques established that the reverse pulse current deposition can generate deposits which increase the corrosion resistance of the anodic film.eng
dc.description.abstractEste artículo presenta los resultados de mejora en las propiedades electroquímicas de películas anódicas de tipo poroso crecidas sobre aleación de aluminio AA2024 T3, obtenidas con las técnicas de corriente continua, corriente continua pulsada y corriente inversa, a través de un electrolito H2SO4 al 15% v/v. Se utilizó el análisis morfológico de microscopía de fuerza atómica y microscopía electrónica de barrido, lo que permitió identificar que las películas obtenidas con pulso de corriente inversa tienen un tamaño de grano menor que las obtenidas por las otras dos técnicas de depósito. Para la evaluación de la resistencia a la corrosión en las películas, se utilizó espectroscopía de impedancia electroquímica y curvas de polarización anódica Tafel. Estas técnicas de evaluación establecieron que la deposición de corriente de pulso inverso puede generar depósitos que aumentan la resistencia a la corrosión de la película anódica.esp
dc.format.extent11 páginasspa
dc.format.mimetypeapplication/pdfspa
dc.language.isoengspa
dc.publisherESGspa
dc.rights© 2013 by ESGeng
dc.sourcehttp://www.electrochemsci.org/papers/vol8/80709607.pdfspa
dc.titleImproved Corrosion Protection Properties in Anodic Films Type Porous on 2024 T3 Aluminium Alloys Obtained by Pulse Reverse Plating.eng
dc.typeArtículo de revistaspa
dc.type.versioninfo:eu-repo/semantics/publishedVersionspa
oaire.accessrightshttp://purl.org/coar/access_right/c_abf2spa
oaire.versionhttp://purl.org/coar/version/c_970fb48d4fbd8a85spa
dc.contributor.researchgroupManufactura y Serviciosspa
dc.publisher.placeBogotá, Colombia.spa
dc.relation.citationendpage9617spa
dc.relation.citationstartpage9607spa
dc.relation.citationvolume8spa
dc.relation.indexedN/Aspa
dc.relation.ispartofjournalInternational Journal of Electrochemical Scienceeng
dc.relation.referencesG. Mable Pinto, J. Nayak, A. Nityananda Shetty, Int. J. Electrochem. Sci., 4 (2009) 1452spa
dc.relation.referencesW. Aperador, J. Caballero-Gómez, A. Delgado, Int. J. Electrochem. Sci., 8 (2013) 6154spa
dc.relation.referencesM. Bethencourt, F.J. Botana, M.J. Cano, M. Marcos, J.M. Sánchez Amaya, L. González Rovira, Corrosion Science, 51 (2009) 518spa
dc.relation.referencesS. Valizadeh, E.B Svedberg, P. Leisner, Journal of Applied Electrochemistry, 27 (2002) 97spa
dc.relation.referencesH. Ashassi-Sorkhabi, A. Hagrah, N. Parvini-Ahmadi, J. Manzoori, Surface and Coatings Technology, 140 (2001) 278spa
dc.relation.referencesH. Chi-Chang, W. Chi-Ming, Surface and Coatings Technology, 176 (2003) 75spa
dc.relation.referencesA. Stankeviciute, K. leinartas, G. bikulcius, D. virbalyte,. Journal of applied electrochemistry,28 (1998) 89spa
dc.relation.referencesJ. Aldykewicz, H.S. Isaac, A.J. Davenport. J. Electrochem. Soc. 142 (1995) 3342spa
dc.relation.referencesW. Bensalah, K. Elleuch, M. Feki, M. Wery, M.P. Gigandet, H.F. Ayedi.. Mater. Chem. Phys. 108 (2008) 296spa
dc.relation.referencesJ.P. Sullivan, G.C. Wood, Proc. Roy. Soc. Lond. 317 (1970) 511–543.spa
dc.relation.referencesS.W. Dean, W.H. Anthony. Degradation of metals in atmosphere. American society of testing and materials, Philadelphia (1988)spa
dc.relation.referencesH.M. Obispo, L.E. Murr, M. Arrowood, E.A. Trillo, J. Mater. Sci, 35 (2000) 3479spa
dc.relation.referencesJ.V. Kloet, A.W. Hassel, M. Stratmann, Z. Phys. Chem. 219 (2005) 1505spa
dc.relation.referencesL. Lacroix, L. Ressier, C. Blanc, G. Mankowski. J. Electrochem. Soc. 155 (2008) 131spa
dc.relation.referencesT.J. Warner, M.P. Schmidt, F. Sommer, D. Bellot. Z. Metallkd. 86 (1995) 494spa
dc.relation.references. P. Campestrini, E.P.M. Van Westing, H.W. Van Rooijen, J.H.W. De Wit. Corros. Sci. 42 (2000) 1853spa
dc.relation.references. J.W. Silva, A.G. Bustamante, E.N. Codaro, R.Z. Nakazato, L.R.O. Hein. Appl. Surf. Sci. 236 (2004) 356spa
dc.relation.referencesG.O. Llevbare. Corrosion. 56 (2000) 227spa
dc.relation.referencesW. Aperador, E. Vera, L. M. Ipaz., Revista EIA, 15 (2011) 9.spa
dc.relation.referencesS. jiang, P. Luo, H.H. Zhou, C. P Fu, Y.F.Kuang, Transactions of Nonferrous Metals Society of China, 18(2008)825.spa
dc.relation.referencesH.Shih, S. Tzou, Surface and Coatings Technology, 124 (2000)278.spa
dc.relation.referencesB. Fori, P. Taberna, L. Arurault, J. Bonino, C. Gazeau, P. Bares, Colloids and Surfaces A: Physicochemical and Engineering Aspects, 415(2012)187.spa
dc.relation.referencesY. Ma, X. Zhou, G.E. Thompson, M. Curioni, X. Zhong, E. Koroleva, P. Skeldon, P. Thomson, M. Fowles, Corrosion Science, 53 (2011) 4141.spa
dc.relation.referencesS. A. Fadl-allah, Q. Mohsen, Applied Surface Science, 256 (2010) 5849.spa
dc.rights.accessrightsinfo:eu-repo/semantics/openAccessspa
dc.subject.armarcPelículas anódicasesp
dc.subject.armarcElectroquímicaesp
dc.subject.armarcElectrochemistryeng
dc.subject.armarcAnálisis electroquímicoesp
dc.subject.armarcElectrochemical analysiseng
dc.subject.proposalpulse currenteng
dc.subject.proposalanodic filmseng
dc.subject.proposalatomic force microscopyeng
dc.subject.proposalelectrochemical impedance spectroscopyeng
dc.subject.proposalTafeleng
dc.type.coarhttp://purl.org/coar/resource_type/c_6501spa
dc.type.contentTextspa
dc.type.driverinfo:eu-repo/semantics/articlespa
dc.type.redcolhttp://purl.org/redcol/resource_type/ARTspa


Ficheros en el ítem

Thumbnail

Este ítem aparece en la(s) siguiente(s) colección(ones)

Mostrar el registro sencillo del ítem